Cefuroxime-Loaded Hydrogels for Prevention and Treatment of Bacterial Contamination of Open Wounds
Table 1
Temperature intervals of weight loss on heating, obtained by the DTA method.
| | Sample | Peak 1 | Peak 2 |
| 1 | D20-g-PAA-0.4 | 35-190 | 315-485 | 2 | D100-g-PAA-0.4 | 45-160 | 320-450 | 3 | D500-g-PAA-0.4 | 30-180 | 330-450 | 4 | DS500-g-PAA-0.4 | 30-185 | 350-480 | 5 | PAA-0.4 | 35-190 | 300-470 |
|
|