Degradable PHBHHx Modified by the Silk Fibroin for the Applications of Cardiovascular Tissue Engineering
Figure 7
OD values of the human fibroblasts on the SF-modified porous PHBHHx scaffolds at different culture times, with porous PHBHHx scaffold as control: PHBHHx with pore size between 50~75 μm. 0.75% silk fibroin was used for the modification. Error bars represent means ± SD for . * [19].