Research Article
Evaluation of Dynamic Materials Procured from Waste Biomass
Table 2
Thermogravimetric-differential thermal analysis of fiber and composite.
| Sample | TGA | DTA | IDT | FDT | % Residue left | Peaks in °C (μV) |
| H. sabdariffa Hs-g-poly(MA-co-VA) | 225.7 | 463.0 | 20.00 | 139.7 (6), 327.9 (18.0), 422.7 (14) | 289.4 | 540.0 | 16.66 | 146.9 (8), 347.2 (22), 393.9 (28.5) | Phenoplast | 500.0 | 600.0 | — | 551.0 (150) | Hs-r-PF composite | 540.0 | 680.0 | 10.00 | 610.0 (164) |
|
|
IDT: initial decomposition temperature; FDT: final decomposition temperature.
|