Research Article

Synthesis and Characterization of Hydrolysis Grown Zinc Oxide Nanorods

Figure 1

SEM image of the spin-coated seed layer for different ethanolamine concentration with a fixed concentration of zinc acetate at 0.1 M: (a) 0.05 M, (b) 0.1 M, (c) 0.15 M, (d) 0.2 M, (e) 0.25 M, and (f) 0.3 M.
983181.fig.001a
(a)
983181.fig.001b
(b)
983181.fig.001c
(c)
983181.fig.001d
(d)
983181.fig.001e
(e)
983181.fig.001f
(f)