594573.fig.0010a
(a)
594573.fig.0010b
(b)
594573.fig.0010c
(c)
594573.fig.0010d
(d)
Figure 10: Worn surface of composite. (a) Cast at a pressure of 1 MPa at 200 rpm (b) peeling off of the dispersoids resulting in sudden weight loss at high loads (c) aged composite do not show very clear wear tracks (d) at higher pressures.