Fabrication and Degradation of Electrospun Scaffolds from L-Tyrosine-Based Polyurethane Blends for Tissue Engineering Applications

Table 3

Mass loss comparison between thin films and electrospun fibers after 35 days of hydrolytic degradation.

Thin film (%)Spun fiber (%)Increase over film (%)

Blend 116.629.376.3
Blend 211.521.284.6
Blend 38.818.2107.5
Blend 46.312.8102.7
Blend 53.26.398.1