Research Article
Structure and Composition of Ba-W-Ti-O Ceramics Interface Regions Formed at Ultrasonic Vibration
Table 3
The Ti: Ba: W ratio (at.%) in the bulk (XRD data) and interface regions (XPS) of the ceramics investigated.
| Specimen | Method | Ti: Ba: W |
| 1 | XRD | 94.0: 22.0: 1 | XPS | 7.1: 2.7: 1 | 2 | XRD | 31.0: 8.0: 1 | XPS | 7.5: 2.2: 1 | 3 | XRD | 30.0: 8.0: 1 | XPS | 6.0: 2.5: 1 | 4 | XRD | 23.0: 6.0: 1 | XPS | 5.3: 1.8: 1 | 5 | XRD | 38.0: 10.0: 1 | XPS | 5.3: 2.8: 1 | 6 | XRD | 30.0: 8.0: 1 | XPS | 6.6: 1.3: 1 |
|
|