Research Article

Rare Earth-Doped SrTio3 Perovskite Formation from Xerogels

Figure 4

X-ray diffraction patterns of doped strontium titanate samples (a) calcined at 1100°C and (b) sintered at 1350°C.
926537.fig.004a
(a)
926537.fig.004b
(b)