Cyclic voltammogram of POAP at p H = 1 , scan rate, 𝜈 = 0 . 1  V s−1, Pt electrode, electrode area 𝐴 = 0 . 1 2 6  cm2, supporting electrolyte: 0.4 M NaClO4 + 0.1 M HClO4 [10].