Research Article
Friction Performance Optimization of Chemically Deposited Ni-P-W Coating Using Taguchi Method
Table 1
Design factors and their levels.
| Design factors | Unit | Levels | 1 | 2 | 3 |
| Concentration of source of nickel (nickel sulfate solution) (A) | g/L | 20 | | 30 | Concentration of reducing agent (sodium hypophosphite solution) (B) | g/ L | 14 | | 20 | Concentration of source of tungsten (sodium tungstate) (C) | g/ L | 15 | | 25 | Annealing temperature (D) |
°C | 400 | | 600 |
|
|
Initial condition.
|