Research Article

Conductivity and Complex Electrical Formalism of the Iron-Doped PbLaTiO3 Ferroelectric Relaxor

Figure 4

Curie-Weiss law ((a) and (b)) and modified Curie-Weiss law ((c) and (d)) of PLFT ceramics for different temperatures at 10 kHz. Relaxation and diffuseness parameters ((e) and (f), lines are given as eye guides).
231302.fig.004a
(a)
231302.fig.004b
(b)
231302.fig.004c
(c)
231302.fig.004d
(d)
231302.fig.004e
(e)
231302.fig.004f
(f)