Corrosion of WC-VC-Co Hardmetal in Neutral Chloride Containing Media
Table 4
Raman shifts after corrosion in NaCl.
| Specimen | Raman bands | Possible phase | References |
| WC-10C | 133 & 249 | WO3 | [16] | 814.5 | WO3 | [17] | 679 & 958.5 | WO3·2H2O | [16] |
| WC-0.4VC-10Co | 131 | WO3 | [16] | 697 | WO3 | [18] | 813.5 | WO3 | [17] | 881.5 | WO3·nH2O | [19] | 968.5 | WO3·2H2O | [16] |
| WC-10VC-12Co | 131 & 803 | WO3 | [16] | 261 & 962 | WO3·2H2O | [20] |
| WC-27VC-11Co | 132.5, 262.5, 700, & 805.5 | WO3 | [16] |
|
|