Research Article
Fabrication of Hybrid Surface Composite through Friction Stir Processing and Its Impression Creep Behaviour
Table 1
Steady state creep rates in friction stirred zone and base metal (load: 5 kg).
| Temperature (°C) | Steady state creep rate (min−1) | Base metal region | Friction stirred region |
| 30 | 3 × 10−5 | 8.33 × 10−6 | 100 | 30.4 × 10−5 | 8.7 × 10−5 | 150 | 200 × 10−5 | 90 × 10−5 | 180 | 235.7 × 10−5 | 178.9 × 10−5 |
|
|