Research Article

Corrosion Inhibition of Cu-Ni (90/10) Alloy in Seawater and Sulphide-Polluted Seawater Environments by 1,2,3-Benzotriazole

Figure 19

SEM images of Cu-Ni (90/10) alloy in synthetic seawater containing 10 ppm sulphide in the absence ((a): ×3000, (b): ×5000) and presence ((c): ×3000, (d): ×5000) of BTAH for a period of 30 days.
703929.fig.0019a
(a)
703929.fig.0019b
(b)
703929.fig.0019c
(c)
703929.fig.0019d
(d)