Corrosion Inhibition of Cu-Ni (90/10) Alloy in Seawater and Sulphide-Polluted Seawater Environments by 1,2,3-Benzotriazole

Table 16

Elemental composition of Cu-Ni (90/10) alloy obtained by SEM-EDX in seawater and sulphide-polluted seawater in the absence and presence of BTAH after 30-day immersion period.

SeawaterSeawater + 10 ppm sulphideSeawater + 3.33 mM BTAHSeawater + 10 ppm sulphide + 3.33 mM BTAH
ElementAtom (%)ElementAtom (%)ElementAtom (%)ElementAtom (%)

O54.5O39.37C K30.47C K28.58
S0.6S17.34N K4.14N K3.25
Cl1.29Cl2.02O K2.64O K6.51
Fe0.97Fe0.56Fe K0.85Fe K0.87
Ni6.17Ni4.59Ni K7.1Ni K7.81
Cu36.47Cu36.12Cu K54.8Cu K52.98