Research Article

Influence of Nd Substitution by La in on Structural and Transport Properties for Sensing Applications

Table 2

Theoretical fitted parameters below , and maximum %TCR (see Figure 4) with respect to average radius of NLSMO series.

CompositionSample
code
Average radius
Å
(Ω cm)   
(Ω cm K−2)
  
(Ω cm K−4.5)
Maximum TCR% (K−1)

Nd0.7Sr0.3MnO3NLSMO 01.3210.05036 1.40
Nd0.6La0.1Sr0.3MnO3NLSMO 11.3300.02208 2.66
Nd0.5La0.2Sr0.3MnO3NLSMO 21.3390.00341 2.65