Steep suction procedure. Median values of parameters defining the creep extension in the repeat stress-versus-time recording modality (3 and 5 cycles) for different probe aperture diameters (AD 2 mm and AD 4 mm) using a 500 mbar depression for 5 s performed with (w) and without (w/o) outer contention on normal skin and connective tissue disorders. The differences in maximum deformation after 3 and 5 cycles ( MD3, and MD5, and the corresponding residual deformations ( RD3 and RD5) were recorded.

Skin condition MD3 (%) MD5 (%) RD3 (%) RD5 (%)
AD 2 mmAD 4 mmAD 2 mmAD 4 mmAD 2 mmAD 4 mmAD 2 mmAD 4 mm
ww/oww/oww/oww/oww/oww/oww/oww/o

Normal3355457556666677
Scleroderma1122112222343434
Ehlers-Danlos1112345534554555
Dermatoporosis1145224522455595
Acromegaly2253222222542323