Controlled Geometry Formation of the Carbon Coils by the Substrate Pretreatment
Figure 5
FESEM images for the surface morphologies of the samples after 10 minutes deposition reaction for sample E under the magnification of (a) 500, (b) 10,000, and (c) 30,000 and for sample F under the magnification of (d) 500, (e) 10,000, and (f) 30,000.
(a)
(b)
(c)
(d)
(e)
(f)
We are committed to sharing findings related to COVID-19 as quickly as possible. We will be providing unlimited waivers of publication charges for accepted research articles as well as case reports and case series related to COVID-19. Review articles are excluded from this waiver policy. Sign up here as a reviewer to help fast-track new submissions.