Electrochemical Study of Ni20Cr Coatings Applied by HVOF Process in ZnCl2-KCl at High Temperatures

Figure 12

Cross-sectional aspect of the Ni20Cr as-grinded coating and elements distribution after corrosion test at 450°C.