Research Article

Highly Dispersed in Porous Silica for CO Hydrogenation

Figure 3

Changes in the XP spectra of Mo-M-SiO2 in the (a) Mo 3d, (b) deconvoluted spectrum for Mo 3d obtained after treatment at 623 K and (c) at 823 K, (d) C 1s, (e) Si 2p, and (f) O 1s region during carburization in Ar gas; room temperature refers to the untreated sample.
725970.fig.003a
(a)
725970.fig.003b
(b)
725970.fig.003c
(c)
725970.fig.003d
(d)
725970.fig.003e
(e)
725970.fig.003f
(f)