Research Article

Producing Polymer Fibers by Electrospinning in Supercritical Fluids

Figure 2

SEM of PVP fibers created by electrospinning a 5 wt% PVP-DCM solution into N2 at 298 K and (a) 2.5 MPa; (b) 5 MPa; (c) 7.5 MPa, and (d) simulated binary phase equilibrium for N2-DCM and air-DCM solutions.
508905.fig.002a
(a)
508905.fig.002b
(b)
508905.fig.002c
(c)
508905.fig.002d
(d)