Controlling Foam Morphology of Poly(methyl methacrylate) via Surface Chemistry and Concentration of Silica Nanoparticles and Supercritical Carbon Dioxide Process Parameters
Figure 8
(a) Cell density and (b) cell size of the highly fluorinated, high concentration (FF-High) sample processed at 65 and 85°C at saturation pressures 8.97, 13.45 and 17.93 MPa. The error bars show the standard error of five samples.