Research Article

Corrosion and Corrosion Inhibition of High Strength Low Alloy Steel in 2.0 M Sulfuric Acid Solutions by 3-Amino-1,2,3-triazole as a Corrosion Inhibitor

Figure 3

Nyquist plots for the HSLA steel after its immersion for (1) 10 min and (2) 60 min in the 2.0 M H2SO4 solutions, respectively.
538794.fig.003