Research Article

Galvanic Displacement of Gallium Arsenide Surface: A Simple and Low-Cost Method to Deposit Metal Nanoparticles and Films

Figure 7

Effect of inorganic acids on thickness of Au thin films. Galvanic displacement is conducted in 1.0 mM, HAuCl4 solution containing plating bath which includes 0.8 M HCl, 4.6 M H2SO4, or 3.3 M HF for 3 min.
784824.fig.007