Research Article
4-Nitroaniline Degradation by TiO2 Catalyst Doping with Manganese
Table 2
Comparing diffraction angles and intensity of rutile TiO2 standard card and prepared TiO2 doped with manganese.
| Rutile TiO2 Standard card (00-001-1292) | Angle (°) | 27.51 | 36.06 | 39.31 | 41.19 | 44.14 | 54.23 | 56.78 | Intensity | 80 | 60 | 4 | 30 | 12 | 100 | 30 |