Research Article

Parametric Study of Time-Dependent Corrosion Product Activity due to 56Mn, 58Co, and 60Co in the Primary Coolant Circuit of a Typical Pressurized Water Reactor

Table 1

Activated corrosion products and their reaction properties [13].

Corrosion productsReaction and neutron energyActivation cross section and half-life

56Mn55Mn(n, ) 56Mn (En is thermal)13.4 b (2.58 h)9.2 × 1013
58Co58Ni(n, p) 58Co (fast neutrons)0.146 b (70.88 d)9.02 × 1013
60Co59Co(n, ) 60Co20 b (5.3 y)9.02 × 1013