Adsorbability Enhancement of Macroporous Resin by Dielectric Barrier Discharge Plasma Treatment to Phenol in Water

Table 7

Structural properties of the virgin and DBD treated resin.

Resin samples (m2/g) (m2/g) (m3/g) (m3/g)Average pore diameter (nm)

Untreated944.6715.80.3770.5861.428
DBD 11056.4838.90.5930.6581.428
DBD 2937.7605.10.3010.6101.418