Shear stress-shear rate curve of various slurry concentrations (%-1 solid lines represent 0∼120 s−1; %-2 dashed lines represent 120∼0 s−1): (a) 73%∼76% mass concentration; (b) 77%∼79% mass concentration; (c) 80%∼82% mass concentration.