Figure 2

N2 adsorption isotherms at −196°C of parent (P) and samples treated with 1 M NaAlO2 solution at different contact time (A1 = 0.5 h, B1 = 1.5 h, and D1 = 6 h) (a) and NaAlO2 concentration (C1 = 1 M, C1.5 = 1.5 M, and C2 = 2 M) after 3 h treatment (b).