Research Article
Sintering and Hardness Behavior of Fe-Al2O3 Metal Matrix Nanocomposites Prepared by Powder Metallurgy
Table 1
Nomenclature of specimens.
| Sl. no. | Sintering temperature (°C) | Sintering time (h) | Specimen code 5% Al2O3 | Specimen code 10% Al2O3 | Specimen code 20% Al2O3 | Specimen code 30% Al2O3 |
| 1 | 900 | 1 | 5AFe900() | 10AFe900() | 20AFe900() | 30AFe900() | 2 | 1000 | 1 | 5AFe1000() | 10AFe1000() | 20AFe1000() | 30AFe1000() | 3 | 1100 | 1 | 5AFe1100() | 10AFe1100() | 20AFe1100() | 30AFe1100() | 4 | 900 | 2 | 5AFe900() | 10AFe900() | 20AFe900() | 30AFe900() | 5 | 1000 | 2 | 5AFe1000() | 10AFe1000() | 20AFe1000() | 30AFe1000() | 6 | 1100 | 2 | 5AFe1100() | 10AFe1100() | 20AFe1100() | 30AFe1100() | 7 | 900 | 3 | 5AFe900() | 10AFe900() | 20AFe900() | 30AFe900() | 8 | 1000 | 3 | 5AFe1000() | 10AFe1000() | 20AFe1000() | 30AFe1000() | 9 | 1100 | 3 | 5AFe1100() | 10AFe1100() | 20AFe1100() | 30AFe1100() |
|
|