Hybrid Fibre Polylactide Acid Composite with Empty Fruit Bunch: Chopped Glass Strands
Figure 5
Tensile strength of the pure EFB, hybrid EFB-GLS, and pure GLS fibre PLA composite at various % and GLS fibre length produced using chloroform and dichloromethane solvent.