Specification of tests and materials.

Cross-tension test (DIN EN ISO 14273)Lap-shear test (DIN EN ISO 14272)

958501.table.1a958501.table.1b

GFRPCFRPMetal

FiberE-GlasCarbonDeep drawing steel DC04
MatrixPP PA 6
Lay up[0/90][0/90/0/90]
Thickness 1.0 mm1.5 mm1.5 mm
Fiber volume 0.350.55

Manufacturing parameters

Joining point diameter5.3 mm
Flow drill speed3000/min
Joining force2.0 kN
Plasticization diameterGFRP: 20.0 mm, CFRP: 30.0 mm