Resin Composite Materials for Chairside CAD/CAM Restorations: A Comparison of Selected Mechanical Properties

Table 1

Machinable materials used in the study.

BrandAbr.ManufacturerCompositionLot no.ShadeBlock size

Grandio blocsGRVOCO, Cuxhaven, Germany86 wt % nanohybride fillers, 14% UDMA + DMA [15, 16]1711521A2 HTC 14L
Tetric CADTEIvoclar vivaden, Schaan, LiechtensteinDimethacrylates 28.4 wt%: Bis-GMA, Bis-EMA, TEGDMA, UDMA; fillers: 71, 1 wt%, barium glass (<1 um), silicon dioxide (<20 nm) [17]354703M2 HT14
Brilliant criosCRColtene/Whaledent A.G. Altstatten, SwitzerlandResin matrix cross-linked methacrylate, 70.7 wt % barium glass (<1 μm), amorphous silica (<20 nm) [15, 18]H22667A2 LTC 14
Katana avencia blockAVKuray Noritake dental, Tokyo, JapanUDMA, TEGDMA with 62 wt % aluminum filler (20 nm), silica filler (40 nm) [19]000318A2LT12
CerasmartCSGC dental product Europe, Leuven, BelgiumBisMEPP, UDMA, DMA with 71% wt% silica (20 nm) and barium glass (300 nm) [15, 19]37690A3 C14
Shofu block HCHCShofu inc., Kyoto, JapanUDMA, TEGMA, 61 wt% silica powder, micro fumed silica, zirconium silicate [15, 19]071601A2 LT14

UMDA: urethane dimethacrylate; TEGDMA: triethylene glycol dimethacrylate; Bis-GMA: bisphenol A diglycidylether methacrylate; Bis-EMA: ethoxylate bisphenol-A dimethacrylate; DMA: dimethacrylate; Bis-MEEP: 2,2-Bis(4-methacryloxypolyethoxyphenyl) propane; EDMA: ethyleneglycoldimethacrylate; DMA: dimethacrylate.