Research Article

Study on the Microstructure and Texture of 3003 Aluminum Sheets Rolled by Laser-Textured Roll

Figure 3

Polarized optical micrographs of CR rolled 3003 alloy sheets, with the reduction rates of (a) 42 pct, (b) 75 pct, and (c) 90 pct.
587938.fig.003a
(a)
587938.fig.003b
(b)
587938.fig.003c
(c)