Journal of Metallurgy / 2011 / Article / Fig 3

Research Article

Transition in Deformation Mechanism of AZ31 Magnesium Alloy during High-Temperature Tensile Deformation

Figure 3

Nominal-stress-nominal-strain curves for tensile deformation at 523 K (a), 573 K (b), and 623 K (c) at an initial strain rate of to 10−4 s−1.
165307.fig.003a
(a)
165307.fig.003b
(b)
165307.fig.003c
(c)

We are committed to sharing findings related to COVID-19 as quickly and safely as possible. Any author submitting a COVID-19 paper should notify us at help@hindawi.com to ensure their research is fast-tracked and made available on a preprint server as soon as possible. We will be providing unlimited waivers of publication charges for accepted articles related to COVID-19. Sign up here as a reviewer to help fast-track new submissions.