Research Article

Transition in Deformation Mechanism of AZ31 Magnesium Alloy during High-Temperature Tensile Deformation

Figure 8

Optical micrographs of the as-rolled specimens deformed during tensile tests at 573 K (a)–(c) and 623 K (d)–(f), for = 85% (a, d), = 135% (b, e), and = 180% (c, f).
165307.fig.008a
(a)
165307.fig.008b
(b)
165307.fig.008c
(c)
165307.fig.008d
(d)
165307.fig.008e
(e)
165307.fig.008f
(f)