Research Article
Influence of Partial Replacement of Nickel by Nitrogen on Microstructure and Mechanical Properties of Austenitic Stainless Steel
Table 6
Tension results of different steel.
| | Reference steel heat-treated at 1100°C | Reference steel heat-treated at 1200°C | Modified steel heat-treated at 1100°C | Modified steel heat-treated at 1200°C |
| YS stress, MPa | 274 | 253 | 486 | 418 | Ultimate tensile strength, MPa | 552 | 538 | 824 | 752.917 | Elongation % | 57 | 60 | 46 | 55.5000 |
|
|