Review Article

Surface Modification and Alloying of Aluminum and Titanium Alloys with Low-Energy, High-Current Electron Beams

Figure 7

Micrographs of the surface of the Ti-6Al-4V samples, irradiated at RT (a, b), 200 (c) and 400°C (d); (a) laser microscopy, (b, c, d) SEM.
673685.fig.007a
(a)
673685.fig.007b
(b)
673685.fig.007c
(c)
673685.fig.007d
(d)