Research Article

Aging Behaviour of Al-Mg-Si Alloys Subjected to Severe Plastic Deformation by ECAP and Cold Asymmetric Rolling

Figure 6

Morphology of strengthening precipitates detected in (a) solution annealed and peak aged coarse-grained alloy, (b) presolution annealed and peak-aged after 1 ECAP pass, (c) presolution annealed and peak-aged after 6 ECAP passes [13].
959643.fig.006a
(a)
959643.fig.006b
(b)
959643.fig.006c
(c)