Research Article
Influence of Vanadium and Cast Temperature on Nitrogen Solubility of Stainless Steel
Table 2
Interaction parameters in steel melts after Grigorenko and Pomarin [
20].
| Element () | | | |
| V | −363/ + 0.080 | 17.6/ − 0.006 | −0.45/ + 0.00018 | Nb | −237/ + 0.055 | 5.14/ − 0.0018 | | Cr | −167/ + 0.042 | 3.3/ + 0.0010 | −0.039/ + 0.000012 | Ta | −102/ + 0.018 | | | Mn | −73/ + 0.022 | 0.80/ − 0.00038 | | Mo | −34/ + 0.0061 | | | W | −3.6/ + 0.0039 | | | Ni | −18.4/ + 0.00042 | | | Si | 171/ − 0.031 | | | C | 274/ − 0.060 | −28/ + 0.035 | | O | 1640/ − 1.14 | | | N | 320/ − 0.12 | | |
|
|