587265.fig.004a
(a)
587265.fig.004b
(b)
Figure 4: Observed profile (points), calculated profile (the solid line), and the profile difference above for the Rietveld patterns of Al-11Si-11Fe melt spun (a) and annealed at 350°C/25 h (b) alloys.