Conversion of Mill Scale Waste into Valuable Products via Carbothermic Reduction
Figure 9
Variation of (a) sulphur content and (b) desulfurization degree of the metal, using 500 gm of CaO-CaF2 (4 : 1) in the furnace with adding 250 gm of different fluxing type in the mold, (1) zero, (2) CaO + CaF2 + FeSi-C, and (3) CaO + CaF2 (4) CaSi.