Research Article

Parameter Optimization in the Synthesis of BZT Ceramics to Achieve Good Dielectric Properties

Figure 6

(a) SEM of the ceramic sintered at 1350°C. (b) HRSEM of ground powders by 4 h.
393017.fig.006a
(a)
393017.fig.006b
(b)