Parameter Optimization in the Synthesis of BZT Ceramics to Achieve Good Dielectric Properties
Figure 8
Dielectric constant of BZT sintered at 1400°C. Inset: zoom for {1–10 kHz} range, : for sample sintered at 1400°C, ▲: for 1350°C sintered BZT, □: dielectric loss for 1350°C sintered BZT, ■: dielectric loss for 1400°C sintered BZT.
We are committed to sharing findings related to COVID-19 as quickly as possible. We will be providing unlimited waivers of publication charges for accepted research articles as well as case reports and case series related to COVID-19. Review articles are excluded from this waiver policy. Sign up here as a reviewer to help fast-track new submissions.