Research Article

Glass Formation in Ni-Zr-(Al) Alloy Systems

Figure 2

XRD patterns of the as-cast Ni67Zr33 melt spun ribbons at different spinning velocities. The inset is DSC curve of Ni67Zr33 melt spun ribbon at 4000 rpm.
575640.fig.002