Research Article

Effect of Deposition Time on the Morphological Features and Corrosion Resistance of Electroless Ni-High P Coatings on Aluminium

Figure 5

Morphology of the corroded sample indicating localised corrosion. (a) Coating deposited for 30 minutes (b) Coating deposited for 180 minutes.