Research Article

Biodegradation Study of Nanocomposites of Phenol Novolac Epoxy/Unsaturated Polyester Resin/Egg Shell Nanoparticles Using Natural Polymers

Table 7

Weight change of the samples due to their water absorption after 14 days’ time (day).

Time (day) Sample
12345678910

1 2.9012.8853.0753.1363.4193.4453.6443.6484.1674.174
22.9022.8873.0783.1393.4373.4633.6723.6954.1854.214
32.9012.8863.0813.1443.4483.4743.6893.7114.2094.236
42.9032.8883.0833.1483.4593.4823.7233.7414.2174.251
52.9032.8893.0863.1523.4613.5013.7363.7694.2354.269
62.9022.8883.0853.1563.4793.5183.7513.7844.2534.287
72.9022.8873.0893.1543.4953.5393.7783.7964.2794.315
82.9032.8883.0933.1593.5063.5543.7953.8134.2924.331
92.9042.8883.0983.1623.5163.5713.8253.8344.3184.347
102.9012.8893.1043.163.5363.5863.8573.8794.3354.371
112.9032.8893.1063.1683.5373.5993.8713.8954.3594.384
122.9032.8883.1083.1693.5383.6043.9323.9644.3624.399
132.9032.893.113.1713.5453.6083.9693.9774.4164.427
142.9052.893.1123.1763.5453.6083.9873.9974.4394.441