Research Article

Investigation of the Physical and Molecular Properties of Asphalt Binders Processed with Used Motor Oils

Table 1

List of asphalt composites.

#CodeAsphalt typeInter. temp./°CInter. speed/HzCRM % UMO % Inter. time/min

1UMONANANANA100NA
2HU-64-NEATPG64-22NANANANANA
3HU-64-190-30-120-3% UMOPG64-2219030NA3120
4HU-64-190-30-120-9% UMOPG64-2219030NA9120
5HU-64-190-30-2-3% UMO-10% CRMPG64-22190301032
6HU-64-190-30-30-3% UMO-10% CRMPG64-221903010330
7HU-64-190-30-120-3% UMO-10% CRMPG64-2219030103120
8HU-64-190-30-2-9% UMO-20% CRMPG64-22190302092
9HU-64-190-30-30-9% UMO-20% CRMPG64-221903020930
10HU-64-190-30-120-9% UMO-20% CRMPG64-2219030209120
11HU-64-190-30-120-10% CRMPG64-221903010NA120
12HU-64-190-30-120-20% CRMPG64-221903020NA120
13HU-64-160-30-120-3% UMOPG64-2216030NA3120
14HU-64-160-30-120-9% UMOPG64-2216030NA9120
15HU-64-160-30-2-3% UMO-10% CRMPG64-22160301032
16HU-64-160-30-30-3% UMO-10% CRMPG64-221603010330
17HU-64-160-30-120-3% UMO-10% CRMPG64-2216030103120
18HU-64-160-30-120-9% UMO-20% CRMPG64-2216030209120
19HU-64-160-30-120-10% CRMPG64-221603010NA120
20HU-64-160-30-120-20% CRMPG64-221603020NA120