Silver Nanoparticles Confined in SBA-15 Mesoporous Silica and the Application as a Sensor for Detecting Hydrogen Peroxide
Figure 6
The voltammetric response of (a) GC to 3 mM ,
(b) Ag-mSBA-15/GC to 0 mM , (c) Ag-mSBA-15/GC
to 3 mM , (d) nm-Ag/GC to 3 mM ,
and (e) bulk Ag to 3 mM . All experiments were
carried out in 0.2 M HAc-NaAc buffer (pH = 5) electrolyte, scan rate: 50 mV·s−1.