Vapor Sensing Using Conjugated Molecule-Linked Au Nanoparticles in a Silica Matrix
Figure 5
Response of gold nanoparticle/10 mL TEOS coated IDEs when exposed to 10 000 ppm DMMP in CS2. The amount of Au nanoparticles was decreased while keeping the TEOS amount fixed. (a) contained 1.25 mg Au NP:10 uL TEOS, (b) contained 0.63 mg Au NP:10 uL TEOS, (c) contained 0.31 mg Au NP:10 uL TEOS, (d) contained 0.16 mg Au NP:10 uL TEOS.